{"@context":"https://schema.org","@type":"Dataset","@id":"https://datagraph.stage.matportal.org/id/dataset/nanoindentation-cusn8ni2-5-imws","name":"Nanoindentation_CuSn8Ni2.5_IMWS","description":"Nanoindentation_CuSn8Ni2.5_IMWS is a MatPortal dataset catalogue entry listed under KupferDigital, catalogued under source association 910c1a74-6a71-4531-a4eb-0b7e4dcbc166. It includes 2 linked resources with formats such as image/bmp, opju, including FEMBau02_CuSn8Ni2_5.bmp, FEMBau02_CuSn8Ni2.5.opju. Keywords include hardness, modulus. Review the linked source for license and reuse conditions. The original short source note was: Data of Hardness and Modulus. It is published in MatPortal by admin for dataset discovery, linked-data browsing, and assistant/RAG indexing.","license":"","keywords":["hardness","modulus"],"creator":"admin","publisher":"[{\"email\": \"\", \"identifier\": \"\", \"name\": \"IMWS\", \"type\": \"\", \"uri\": \"https://ckan.kupferdigital.org/organization/25667935-76d7-4a0f-9028-b67a2bef1599\", \"url\": \"\"}]","accountablePerson":"admin","version":"","url":"https://stage.matportal.org/datasets/nanoindentation-cusn8ni2-5-imws","distribution":[{"@type":"DataDownload","name":"FEMBau02_CuSn8Ni2_5.bmp","encodingFormat":"image/bmp","contentUrl":"https://ckan.kupferdigital.org/dataset/b7f2dc2a-6356-4302-8e3a-b93edec3b390/resource/6e9a56aa-adca-4cad-9bd1-2b6999dc195f/download/fembau02_cusn8ni2_5.bmp"},{"@type":"DataDownload","name":"FEMBau02_CuSn8Ni2.5.opju","encodingFormat":"opju","contentUrl":"https://ckan.kupferdigital.org/dataset/b7f2dc2a-6356-4302-8e3a-b93edec3b390/resource/b73dbcab-daf2-40d9-856f-b6ecefbf28a5/download/fembau02_cusn8ni2.5.opju"}]}